INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Need to find info about "peralumen"? not sure about spelling

Need to find info about "peralumen"? not sure about spelling

Need to find info about "peralumen"? not sure about spelling

(OP)
Hi everybody,

Has anybody heard of "peralumen"? not sure of the spelling, I think it might be an aluminium alloy, what I am looking for is details strength and properties of the material.

Does anybody out there know about it or know where I can find information about it?

Thank you very much in advance for your help.

gg

RE: Need to find info about "peralumen"? not sure about spelling

I'm not familiar with the details, but I've seen several references to "Peralumin". A Google on that may help

Good Luck
johnwm

RE: Need to find info about "peralumen"? not sure about spelling

Hi,

PERALUMAN (not peralumEn and not peralumIn) is an aluminum alloy.  There are different grades of peraluman such as Peraluman - 300 (AlMg3), Peraluman - 460 (AlMg4.5) and so on.  You can go on the following website to find info on Peraluman - 300, and if you do a search on www.google.ca you'll find more info.

http://www.alcan-sc.com/downloadables/English_datasheets/pe300.pdf

Good luck

Coka

RE: Need to find info about "peralumen"? not sure about spelling

(OP)
Thank you both very much found what I needed.

Always grateful for sites like this and people like you.

gg

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources