INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Chemistry of G-X 300 Cr Mo153

Chemistry of G-X 300 Cr Mo153

Chemistry of G-X 300 Cr Mo153

(OP)
I shall be thankful if someone can give me the chemistry of this alloy. I hope I have got the alloy name correct.
Thanks in anticipation.

RE: Chemistry of G-X 300 Cr Mo153

arunmrao,

check out this web site:
http://www.esterer-guss.de/Wurzen/Qualitaeten-Werkstoffe.html

It is in German, but from what I understand, the chemistry is the following:
3C-0.7Si-0.5Mn-15.5Cr-0.5Ni-1.5Mo-other.

The spelling is actually G-X 300 CrMo 15 3, so if you do a research on www.google.ca, you'll get the website mentioned above as well as some other useful links.

Good luck.  

Coka

RE: Chemistry of G-X 300 Cr Mo153

(OP)
Thanks Coka. I did get to the site you mentioned,but I seemto have missed it. This was the easier way out to get a reply. Star to you.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources