[b]Latent heat of Hastelloy X[/b]
[b]Latent heat of Hastelloy X[/b]
(OP)
What is the latent heat of fusion of the nickel superalloy Hastelloy X?
I know specific heats up to about 1100 celsius, and I can use trendline extrapolation to find ones at temps up to 1260-1355 C (melting range) if I want. But I haven't been able to find any data on latent heat for this material.
I know specific heats up to about 1100 celsius, and I can use trendline extrapolation to find ones at temps up to 1260-1355 C (melting range) if I want. But I haven't been able to find any data on latent heat for this material.