ASTM A510
ASTM A510
(OP)
Can someone provide me with the yield strength of carbon wire steel
Thanks
Thanks
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: ASTM A510
Wires for this specification do not have mechanical properties other than those specified by the purchaser. The chemical composition and dimensional properties are the controlling factors in manufacture of this product.
ASTM A 510 refers you to ASTM A 370 (and several other ASTM standards) for the types of metallurgical tests used to determine mechanical properties of a given wire type.