HT properties of brick mortar
HT properties of brick mortar
(OP)
Can anyone tell me how to find thermal conductivity, density, and specific heat of common mortar used in brick walls?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
HT properties of brick mortar
|
RE: HT properties of brick mortar
Thermal conductivity = .72 W/m K
Density = 1860 kg/m^3
Specific Heat = 780 J/kg K
I assume that the references in this book could also point you to more information about other building materials.