Allowable Contact Stress - Aluminium Sprocket
Allowable Contact Stress - Aluminium Sprocket
(OP)
I have used the hertzian line contact formula to arrive at a contact stess between an aluminium sprocket & steel roller chain.
For a steel sprocket, I have read that a good rule of thumb for the max allowable stress (for 10^8 cycles) = 2.76HB-70MPa (where HB = Brinell hardness).
Does anyone know of a similar rule of thumb for aluminium?
The grade of alum I'm looking at is A380 (LM24 to any Brits)
Thank you, Alan
For a steel sprocket, I have read that a good rule of thumb for the max allowable stress (for 10^8 cycles) = 2.76HB-70MPa (where HB = Brinell hardness).
Does anyone know of a similar rule of thumb for aluminium?
The grade of alum I'm looking at is A380 (LM24 to any Brits)
Thank you, Alan