INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AWS D1.1/D1.1M

AWS D1.1/D1.1M

AWS D1.1/D1.1M

(OP)
Has anyone purchased the AWS D1.1/D1.1M for 2004?  What is the purpose of the "M" in D1.1M?  Is the D1.1M essential?
Is the D1.1 alone sufficient?

I don't like to be cheap.  But I don't like to spend an extra $200 if not necessary.

Any comments?

Thank you!

RE: AWS D1.1/D1.1M

M - Metric

RE: AWS D1.1/D1.1M

D1.M denotes metric units inclusive to the code (similar to ASTM A 6/A 6M).

There are a few changes between the 02 and 04. The most notable being:
*Text is revised to clarify the Engineer's approval requirements.
*CV power supplies are now required for GMAW/FCAW.
*Additional prequalified material specifications.
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources