INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Overlay weld on tubesheet of a heat exchanger

Overlay weld on tubesheet of a heat exchanger

Overlay weld on tubesheet of a heat exchanger

(OP)
In Section VIII Div 2 Part UCL, the Code reads rules in UCL shall apply to vessel which has over lay weld.
If the tubesheet of a heat exchanger is going to be over lay welded to enhance seal weld reliability of tube to tubesheet joint, is the Part UCL still governing?

RE: Overlay weld on tubesheet of a heat exchanger

Why should not? Can you be more specific on your concerns?
The rules in UCL are specific for cladding fabrication and examination, all the rest of design and fabrication rules remains applicable.
Also note that you are referring to Div.1, not Div.2.

prex

http://www.xcalcs.com
Online tools for structural design

See http://www.xcalcs.com/docs/symbolinfo.htm if you want to use symbols on these forums

RE: Overlay weld on tubesheet of a heat exchanger

(OP)
Thank you, prex.
Yes, you are right. It is Div 1, not Div 2.
And I feel my question was a little out of my intention.
What I want know is that isn't there any ground to escape from rules in UCL. After all, we want to weld over lay not in accordance with ASME Section IX, still keeping ASME conformance of the heat exchanger, if ever possible.

RE: Overlay weld on tubesheet of a heat exchanger

Can't see how you could justify that.
After all the main requirements for a non resistant weld overlay cladding are intended at checking that the weld overlay does not impair the resistance of the base material, and of course you can't escape this issue.

prex

http://www.xcalcs.com
Online tools for structural design

See http://www.xcalcs.com/docs/symbolinfo.htm if you want to use symbols on these fora

RE: Overlay weld on tubesheet of a heat exchanger

kyong

You state you wish to comply with the Code. You must observe it ALL,you are not permitted to pick and choose.

Read U-2(b),UW-28,UW-29,UCL-30,UCL-40

RE: Overlay weld on tubesheet of a heat exchanger

(OP)
Thank you, prex and deanc.
I agree with you guys. I think I have to give up trying to justify not following part UCL.

kyong


Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources