Chemical Analysis Oil N0 6
Chemical Analysis Oil N0 6
(OP)
I am looking for chemical analysis , heating value etc
for Bunker Oil ( Oil No 6).
for Bunker Oil ( Oil No 6).
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Chemical Analysis Oil N0 6
|
RE: Chemical Analysis Oil N0 6
For example, http://www.bpmarine.com/default.asp?p=173, http://www.chevrontexaco.com/brands/prodserv/marine.asp, http://www.chevrontexaco.com/brands/prodserv/marine.asp or visit one of the test houses web sites such as FOBAS, Lintech, Viswalab etc. They are able to advise on fuel oil quality in some detail. e.g. www.viswalab.com, http://www.dnv.com/maritim... .
RE: Chemical Analysis Oil N0 6
RE: Chemical Analysis Oil N0 6
But what is "Perry" ?
RE: Chemical Analysis Oil N0 6
RE: Chemical Analysis Oil N0 6
No. 6 oil Btu content - depending on how accurate you need it to be - the best way is to have a fuel analysis done and then use Perry's Chemical Handbook to calculate BTU's (if the analysis did not state it) or from Handbooks :
No.6 Oil Gross Heating value
18,126 Btu/Lb
153,120 Btu/Gal
RE: Chemical Analysis Oil N0 6
No 6 Bunker oil, what is the specific gravity of the oil you intend to use as the heating value differs from 18,790 BTU/LB to 18,540 BTU/LB and the Deg API is from 15 to 10.
??????
R
NOx
RE: Chemical Analysis Oil N0 6