INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Looking for help with an adhesive

Looking for help with an adhesive

Looking for help with an adhesive

(OP)
I need some help in finding a source of an adhesive identical to what is used in fly ribbon.  I believe it is a petroleum base that adheres to paper.  It needs to be sticky enough to hold insects, but allows paper to be seperated from itself if it is glued together.  I have no background with adhesives, so any guidance would be appreciated.

Rich.....

Richard Nornhold, PE
nornrich@redrose.net

RE: Looking for help with an adhesive

I believe the insect strips are often coated with very viscous polybutene or polyisobutylene.  BASF makes them or you could find them via Goggle.

Regards,

Tom Quinn
Adherent Laboratories
www.adherentlabs.com

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources