INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

how to separate particles

how to separate particles

how to separate particles

(OP)
I have glass microspheres which are in wide size distribution, i.e. 10-100um.  Do you have any way to separate the large ones from small ones since I want to narrow the size distribution? Any suggestion is appreciated.

RE: how to separate particles

Try doing a search on "Elutriation".

RE: how to separate particles

(OP)
Dear unclesyd, thanks for your information. I have tried to search the topic on "Elutriation", but i could not find any method practical to me.  I also learned Screener is one equipment for this purpose. But our institute has no this facility. And I only have samll amount of sample. Is there any practical and easy methods to separate them?

RE: how to separate particles

Presumably your "um" unit is microns.  You can screen down to about 25 micron (600 mesh) using an 8" test sceen from tyler or one of the other test sieve manufacturers.  Below this you may need to cyclone.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources