RE: What is the density of Schedule 40 PVC?
ABS 1020 kg/cubic meter
ABS PC 1070 kg/cubic meter
PVC Rigid 1300 kg/cubic meter
PVC 0.007 Plasticized 1290 kg/cubic meter