Cooper + Galvanized pipes
Cooper + Galvanized pipes
(OP)
What is the reaction between a cooper pipe and a galvanized pipe, there is a problem in this kind of connection.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Cooper + Galvanized pipes
RE: Cooper + Galvanized pipes
Do a web search for "galvanic corrosion" to learn the basics.