Corrosion
Corrosion
(OP)
What is the best way to avoid corrosion in a Pipeline that contains H2s around 60,000 ppm , sour water,sour gas,,high temps around 40 c and higher,with high pressures 300 to 1500 psi. Batch program or continous?No Co2 so to mention.





RE: Corrosion
RE: Corrosion
RE: Corrosion