Weldability of A496 Bars
Weldability of A496 Bars
(OP)
ASTM A496 deformed bars are used to make deformed welded wire fabric. It has been my experience that A706 bars are difficult to find when welding of concrete reinforcing is required. Can A496 bars be efectively substituted for A706 bars?