INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

How pressure influence powder when spay drying

How pressure influence powder when spay drying

How pressure influence powder when spay drying

(OP)
I have 2 kind of powders (SiC and Al2O3) mix together become nano-composite powder.
Powders used were alumina/silicon carbide (Al2O3/SiC) nanocomposite powders.  Ultra fine SiC powder and High purity Al2O3 were mixed in distilled water for 24 hours with Alumina balls, then the mixture was filtered and subsequently washed with distilled water to take out alumina balls. The washed mixture was sprayed by EYELA spray dryer SD-1000, received Al2O3/SiC nanocomposite powders.
That powder will be used as feedstock of plasma spray machine. When operating, I saw that speed of powder was not stable. I do not know why?
May be the size of particle of powder was too small, and lack of binder.
I thinhk I can increase particle size of powder by adjust parameters when operating Spray drying machine (such as: temperature, pressure...).
But I don't know how pressure influence particle size of powder when spray drying.
If anyone know this problem, please show me. I really need.
Thank you alot.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources