INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Need supplier info for SMAW electrodes

Need supplier info for SMAW electrodes

Need supplier info for SMAW electrodes

(OP)
I work in a steel mill, and we received a shipment of scrap listed as "Monel plus flux".  Upon inspection, it was obvious they were SMAW electrodes, of various diameters and suppliers.

Our concern is that the flux covering may adversely affect our slag chemistry in our electic arc furnace.  A search of the web got me in contact with one of the electrode manufacturers and I obtained the composition of the flux.  

However, there are also electrodes coded "AGA X-56 ENICU-4".  The electrodes have a black flux covering.  I immediately thought of AGA-Linde Gas as the supplier manufacturer, but a call to them revealed that they no longer manufacture welding electrodes.  I need to find out the composition of the flux covering.  Can anyone help me determine the origin of these rods?  A contact number at the manufacturer would be extrememly helpful.  Thanks in advance.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources