Difference btn Bitumen/Heacy oil/Petroleum/crud oil & tar sand?
Difference btn Bitumen/Heacy oil/Petroleum/crud oil & tar sand?
(OP)
Hi friends!
Can you help me to clear my doubt? What is the difference between Bitumen/Heacy oil/Petroleum/crud oil & tar sand?
According to me,
1) Bitumen (extra heavy oil) found in tar sand(oil sand) deposits.
2) Bitumen: API gravity<= 10
Viscosity > 10,000 cP
Heavy Oil: API gravity <= 20
Viscosity < 10,000 cP
Where is petroleum and crude oil in this category?
Bitumen is found in petroleum or in tar sand?
Any comment is appreciated!
regards,
chem55
Can you help me to clear my doubt? What is the difference between Bitumen/Heacy oil/Petroleum/crud oil & tar sand?
According to me,
1) Bitumen (extra heavy oil) found in tar sand(oil sand) deposits.
2) Bitumen: API gravity<= 10
Viscosity > 10,000 cP
Heavy Oil: API gravity <= 20
Viscosity < 10,000 cP
Where is petroleum and crude oil in this category?
Bitumen is found in petroleum or in tar sand?
Any comment is appreciated!
regards,
chem55





RE: Difference btn Bitumen/Heacy oil/Petroleum/crud oil & tar sand?
John