INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Exhaust header fatigue analysis

Exhaust header fatigue analysis

Exhaust header fatigue analysis

(OP)
I would like to use FEA to get a handle on the life expectancy of a cast stainless steel collector used on an exhaust header for light trucks and SUVs.  Will I need to consider inputs from both the suspension of the vehicle and the engine or just the suspension?

RE: Exhaust header fatigue analysis

You will need to consider vehicle G levels (pot holes, etc...),engine vibration, and thermal expansion. Most of the exhaust failures I have seem were due to thermal expansion. Good luck.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources