stress-strain curve
stress-strain curve
(OP)
Dear friends
Hi
I'm working by ansys 5.4
I want to draw stress-strain curve for ST37 (mild steel).
Dose any body have this curve? If it is "2 or 3 or 4linear" , it's enough.
Thanks a lot
alif
Hi
I'm working by ansys 5.4
I want to draw stress-strain curve for ST37 (mild steel).
Dose any body have this curve? If it is "2 or 3 or 4linear" , it's enough.
Thanks a lot
alif





RE: stress-strain curve
Here is the bi-linear engineering stress strain data.
STRESS STRAIN
36 KSI 0.0012
59 KSI 0.001966666
fsi