INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

how to join 2 mm aluminium plate

how to join 2 mm aluminium plate

how to join 2 mm aluminium plate

(OP)
im building a speaker type solar cooker using aluminium plate and i don't know the best way to join them i've tried to weld them with TRG GAS but it's really hard to do and i don't know how to join them together

RE: how to join 2 mm aluminium plate

tamingsari,
It is difficult to weld aluminium. You need an inert gas environment to do any electric welding. This should be done by a specialist in TIG/MIG welding.
Another way of connecting 2 plates of aluminium are bonding (maybe you need a special type if the temeperature gets too high) or riveting.
Using rivets is probably the easiest way.
Hope this was helpful,
Jelto

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources