INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

I need precast concrete solutions for bridges between 5 and 10 m span

I need precast concrete solutions for bridges between 5 and 10 m span

I need precast concrete solutions for bridges between 5 and 10 m span

(OP)
I would like to know some precast concrete systems for bridges between 5 and 10m span. Here in Spain we are very use to work with precast abutments plus precast beams, but I am looking for a global system for these small bridges (It means only one piece) Do you have some idea???
Thank you
Carlos

RE: I need precast concrete solutions for bridges between 5 and 10 m span

For spans less than 10m you may use single slab with voids.
for 10m the depth of the structure will be less than 1m.
Note: 1m using British Design Loads

RE: I need precast concrete solutions for bridges between 5 and 10 m span

In the US, Conspan and Oldecastle Precast Concrete have precast systems in this span range. You can find them on the web. Sorry, I don't recall the URL.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources