INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Hi, Refer to API 1104, 6 Qualifi

Hi, Refer to API 1104, 6 Qualifi

Hi, Refer to API 1104, 6 Qualifi

(OP)
Hi,
Refer to API 1104,
6 Qualification of Welders,
6.2 SINGLE QUALIFICATION
6.2.2 Scope
c. A change of filler-metal classification from Group 1 or 2 to Group 3 or from Group 3 to Group 1 or 2 (see Table 1)

So, if a welder carried out a test using Group 1 filler, did he qualified for Group 2?

How about Group 4, 5, 6, 7, 8 & 9? If the welder carry out using filler Group 4 to 9, did he only qualified for the tested filler or for all Group?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources