looking for equivalent to Rycut 40AX
looking for equivalent to Rycut 40AX
(OP)
anyone have a supplier for chromoly steel bar which is similar to rycut40ax? T @ 103ksi, Y @93, E @ 19%, machinability @ 100.
thanks,
chip
thanks,
chip
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
looking for equivalent to Rycut 40AX
|
looking for equivalent to Rycut 40AXlooking for equivalent to Rycut 40AX(OP)
anyone have a supplier for chromoly steel bar which is similar to rycut40ax? T @ 103ksi, Y @93, E @ 19%, machinability @ 100.
thanks, chip Red Flag SubmittedThank you for helping keep Eng-Tips Forums free from inappropriate posts. Reply To This ThreadPosting in the Eng-Tips forums is a member-only feature.Click Here to join Eng-Tips and talk with other members! |
ResourcesWhat is rapid injection molding? For engineers working with tight product design timelines, rapid injection molding can be a critical tool for prototyping and testing functional models. Download Now
The world has changed considerably since the 1980s, when CAD first started displacing drafting tables. Download Now
Prototyping has always been a critical part of product development. Download Now
As the cloud is increasingly adopted for product development, questions remain as to just how cloud software tools compare to on-premise solutions. Download Now
|
RE: looking for equivalent to Rycut 40AX
Happy Trails,
Jeannie
RE: looking for equivalent to Rycut 40AX
as for suppliers that depends on where you are.
nick
RE: looking for equivalent to Rycut 40AX
RE: looking for equivalent to Rycut 40AX
Jesus is THE life,
Leonard
RE: looking for equivalent to Rycut 40AX
Don’t know the significance of the AX suffix. The producer, Ryerson Steel (now Ryerson Tull), no longer shows any RYCUT 40 in their stock list:
http://www.ryersontull.com/stocklist/Red...
RE: looking for equivalent to Rycut 40AX
St. Louis Cold Drawn, Inc.
1060 Pershall Road
St. Louis, MO 63137 USA
Jack Webster - Manager of Sales
800.421.9320 phone
314.867.4304 fax
LaSalle Steel
http://www.suppliersonline.com/supplier/...