INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

PH 17-4 CONDITION 1150; tensile strength at 450 deg. F.

PH 17-4 CONDITION 1150; tensile strength at 450 deg. F.

PH 17-4 CONDITION 1150; tensile strength at 450 deg. F.

(OP)
Hello Fellows:

Does anyone have the info on mechanical properties on PH 17-4 Stainless steel Condition H1150 Single stage at 450 deg. F. ?   I need the Tensile strength and the charpy numbers.
Please post or email them to me at akimiadi@nova-technology.com.

I appreciate your help on this matter.

Regards,
Armanto

Alpha

RE: PH 17-4 CONDITION 1150; tensile strength at 450 deg. F.

(OP)
THANKS TVP:

Those web pages sure help me a lot.

Regards,

Armanto

Alpha

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources