INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

A217 grade C12A

A217 grade C12A

A217 grade C12A

(OP)
I need the chemical makeup of this new chrome moly alloy. It is not listed in our set of ASTM info. We are trying to compare it to grade P91
Regards
Tim Holmes

RE: A217 grade C12A

A217 C12A is the cast version of P91 alloy.
It is UNS # J84090.  I believe it is also included in ASME Section IX per the coming 2003 addenda.
Chemical composition per ASTM is
.08-.12 C
.30-.60 Mn
.03 max P
.01 max S
.20-.50 Si
.40 max Ni
8.0-9.5 Cr
.85-1.05 Mo
.060-.10 Cb
.030-.070 N
.040 max Al
.18-.25 V

90-115 ksi tensile
60 ksi min yield
18 elong
45 ROA

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources