INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Where can I find the Thermal Conductivity of Concrete?

Where can I find the Thermal Conductivity of Concrete?

Where can I find the Thermal Conductivity of Concrete?

(OP)
Where can I find the Thermal Conductivity of Concrete? And Linoleum if possible?

RE: Where can I find the Thermal Conductivity of Concrete?

The PCI Design Handbook lists some values. The values vary by unit weight between about 20 and 100 (Btu-in) per (hr)(sq ft of area) per inch thickness. See table 9.1.4 of 5th Edition handbook.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources