INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

silicon-backed elastic in garments

silicon-backed elastic in garments

silicon-backed elastic in garments

(OP)
Can any one tell me about silicon backing used in ladies garments? It looks and feels like the silicon gel you use to seal sinks etc. But it is obviously robust and permanent and can cope with machine wash etc. I would like to know about the material and how it is applied to a fabric /elasticated fabric. Many thanks.Opticsman

RE: silicon-backed elastic in garments

WACKER has a special brochure about textile applications of silicones including this one. It is usually a liquid silicone rubber. Try at www.wacker .com

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources