Titanium/exotic metals dust/fume exposure
Titanium/exotic metals dust/fume exposure
(OP)
I need a solution for my workshop. We fabricate Titanium spools and other exotic metals. I need to be able to minimise my employees exposure to the fumes and dusts created by cutting and grinding and how to clean/dispose of the dusts safely.





RE: Titanium/exotic metals dust/fume exposure
Can you sell titanium dust?
Tom
Air Filtering Equipment
Equipment Choices
You can start as I did with a simple fan and a metal stovepipe. This is very easy and cheap to install. The drawback is that it usually sucks a lot of warm air out during cold weather.
Consultants
Most states provide free consulting. If you are in British Columbia then you can contact the Workers’ Compensation Board at (604) 276-3209.
Three Excellent Articles
1. One is by John Ashe of AAF (American Air Filter) International in Louisville, KY. (305) 443-9353. His article is Controlling Welding Fumes in the July, 1997 issue of The Fabricator. Reprints of the article are available by calling (800) 477-1214 and asking for reprint # APC-4-905.
2. Another good article was in the December 1996 issue of the same magazine. It was written by Joe Topmiller who is Director of Technical support for United Air Specialists at (800) 551-5401 in Cincinnati, Ohio. The article is Addressing Air Quality Issues in the Workplace.
3. The third article is on new respiratory standards by Jay G. Mears in Modern Woodworking. (248) 244-6439. It was called: Intelligence Report: Getting Ready for 42 CFR part 84 call MSA and is available at (888) 867-0602.
Equipment Suppliers:
1. AAF International (American Air Filters) –(305) 443-9353 – small line but appropriate for most shop applications – great technical support – (see articles section above). Excellent technical advice.
2. Abicor Binzel (301) 846-4196 Frederick, MD - They only supply fume extraction guns for welding. Great product if you need it.
3. Airflow Systems (214) 503-8008 Dallas, TX – wide variety of units, overhead units, downdraft tables, and portable units – “Dust and fume Exhaust” pamphlet has good technical information. Recommended for literature.
4. Coppus (508) 756-8391 Millbury, MA – unique, portable dust collection systems – also employee coolers for hot areas. Unique products.
5. Dust Vent, Inc. (630) 543-9007 Addison, IL. – Wide range of equipment and good literature. Recommended for literature.
6. Eurovac (905) 850-9828 in Ontario. –Central vacuum cleaner systems and other dust collection equipment.
7. Farr Pollution Control Products (800) 479-6801 Los Angeles, CA. – Overhead cleaning with or without arms.
8. Gardner Environmental Products (414) 485-4303 Horicon, WI –Ceiling mounted and portable units.
9. Industrial Ventilation Group (800) 610-6010 Harbor Springs, MI –Central and portable units, downdraft tables. Recommended for literature.
10. Lincoln Electric (216) 481-8100 –Offers a central collection system and portable units –just one mention in their catalog.
11. MAC Equipment, Inc. (800) 821-2476 – Huge, complete catalog. Excellent information, great source to build your own system. Recommended for literature.
12. Nederman (313) 729-3344 Westland, MI –Nice literature –looks like nice overhead arm extraction equipment –good information on Do It Yourself. Recommended for literature.
13. Plymovent (732) 417-0808 New Jersey –good equipment –great free booklet “My Pocketguide to Clean Fresh Air”. Recommended for literature.
14. Sly, Inc. (216) 891-3200 Cleveland, OH –Shop size central collection systems to huge industrial systems. Recommended for literature.
15. Trion (800) 421-3956 Greensboro, NC –Overhead units –they advertise a free clean air guide.
16. United Air Specialists (800) 551-5401 Cincinnati, Ohio –Invented the original smoke eaters for bars, etc. –Good equipment –good literature and great technical help. Recommended for literature.
RE: Titanium/exotic metals dust/fume exposure
I don't know if already took care of titanium project but offer the following.
Two years ago I involved with selecting APC unit to control Titanium grinding process. We looked at both wet and dry APC systems to control process and decided on a wet system. We went wet because of dust temperature coming off 250 HP dry type grinder was about 22-2300 deg F and space allocated for control system was small.
The first control device installed was a low pressure wet collector/scrubber and pasted through submicro particulate from the start. Unit was sent back to vendor. The next step was to starting looking at wet ESP or high pressure drop scrubber to control sub micron particualte. We pilot operated a TRI-MER CCS cloud chamber scrubber and found it would handle submicron particulate and worked at about 1-2" of pressure.
TRI-MER Phone is 989 723 7838
Regards,
Mike Claffey