INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Polyurethane Foam?

Polyurethane Foam?

Polyurethane Foam?

(OP)
Hi,
I'm doing a bit of research but unfortunately haven't been able to find a simple answer to this question.
What are the key components in Polyurethane Foam?  I realize that foam is made up of different monomers to make the polymer but I'm still a bit confused.
Any help would be appreciated!

Thanks!
BiodieselChem

RE: Polyurethane Foam?

Polyurethane foams are usually made by the reaction of a polyol with methylene diphenyl diisocyanate (MDI) or toluene diisocyanate (TDI).  Take a look a the following link

http://www.polyurethane.org

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources