INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Thermal cycling analysis with residual stress.

Thermal cycling analysis with residual stress.

Thermal cycling analysis with residual stress.

(OP)
Hi guys,

I'm relatively new to this forum, and I need your help with a problem.

I’m working in the semiconductor industry and I have an analysis that involves simulating the assembly process of a flip chip. I basically need to stress my model with:

1) Reflow (say above 220DegC)
2) Cooling to room temp and recording the residual stress
3) Thermal cycling and recording the deformation and stress at various intervals (50cycles, 500 cycles, 1000 cycles etc)

It would be a big help if anyone can give me a few pointers on how to go about extracting residual stress and stress/strain at thermal cycling intervals. I model both in APDL and interactive mode, but I am more comfortable applying loads in interactive mode.

Thank you all for your help in advance! =)

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources