INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Welding 7075 aluminum

Welding 7075 aluminum

Welding 7075 aluminum

(OP)
Can 7075-T6 aluminum alloy be welded?  If so, by what process?

Thanks.

RE: Welding 7075 aluminum

7075 is one of the "difficult" to weld Al alloys.

I do know it is RSW regularly in the aerospace industry. It can be GTAW, but this process still requires some attention as it tends to crack if welding parameters are not dialed in and adhered to. It has a VERY narrow weldability range.

The welding engineer at one of the companys I worked for years ago told me something about corrosion susceptibility (with regards to our shielding gas and filler metal). Back then I had no clue what he was talking about, but it stayed in my hard drive and years later I now understand his statement.

RE: Welding 7075 aluminum

Sorry, I almost forgot. Contact the very knowledgable people at Alcotec. They are the source for Al welding IMHO.

http://www.alcotec.com/

Good luck.

RE: Welding 7075 aluminum

(OP)
Thanks for the info.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources