INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What is St 37.0?

What is St 37.0?

What is St 37.0?

(OP)
I'm trying to find out the EN designations of a few steel types from the old DIN norm but one of them I just can't find - and actually never heard of.
I know St 37 becomes S235, but what is St 37.0? Is it the same as St 37?

RE: What is St 37.0?

St 37.0 is essentially the same as St 37.  The Werkstoff Nummer is 1.0254.  This grade appeared in DIN 1626, DIN 1629, DIN EN 10216-1 (Draft version), and DIN EN 10217-1 (Draft version).  It was also called P235T1.  The composition is as follows:

C = 0.17 max
P = 0.040 max
S = 0.040 max
N = 0.009 max

RE: What is St 37.0?

(OP)
Thanks for your help!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources