INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Thermal conductivity value for SA-214 STHE Tubes

Thermal conductivity value for SA-214 STHE Tubes

Thermal conductivity value for SA-214 STHE Tubes

(OP)
Dear friends,

What is the thermal conductivity value for SA-214 STHE Tubes?(100 to 212eg F)
Any relevant websites please.

Thanks in advance.

RE: Thermal conductivity value for SA-214 STHE Tubes

According to my old TEMA book, 30 (BTU/hr-ft-Deg F) is about right.  

RE: Thermal conductivity value for SA-214 STHE Tubes

(OP)
Dear speco,

Thanks. I also got the same value. Any relevent websites.  

RE: Thermal conductivity value for SA-214 STHE Tubes

(OP)
Dear speco,

Thanks for your efforts.Useful site.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources