INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Modelling of Composite Bonded Joints

Modelling of Composite Bonded Joints

Modelling of Composite Bonded Joints

(OP)
Does anyone have any useful publications or benchmark examples for conducting detailed finite element modelling of composite bonded joints. Any MSC Nastran exercises would be particularly useful.

Regards
Kieron.

MBDA UK Ltd

RE: Modelling of Composite Bonded Joints

Kieron, we model our laminate build up's on our proprietary software, however it analyses the ply build up, and ply stresses, and determines ply margins of safety, based on a Tsai-Hill calculation. It utilises NASTRAN load conditions.
Is it ply behaviour your looking at modelling?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources