Why SA-182 F317L isn't in B16.5 flange rating tables
Why SA-182 F317L isn't in B16.5 flange rating tables
(OP)
Does any one know why SA-182 F317L isn't listed in B16.5 1998 Table 1A (List of material specifications)?
I am guessing that I could use the Pressure/Temperature ratings for Material Group 2.3, which includes 316L and 304L.
Any insight would be appreciated.
Thanks
Dave
PS: the vessel design conditions are 75 psi @ 750 deg F
I am guessing that I could use the Pressure/Temperature ratings for Material Group 2.3, which includes 316L and 304L.
Any insight would be appreciated.
Thanks
Dave
PS: the vessel design conditions are 75 psi @ 750 deg F





RE: Why SA-182 F317L isn't in B16.5 flange rating tables
http://www.albertaboilers.com/IB&Index/IB03-005.pdf
RE: Why SA-182 F317L isn't in B16.5 flange rating tables
I have been informed that F317 will be added to both B16.5 and B16.34 in the next publication. The other materials have been added to the subcommittee's agenda, and will probably take a little bit longer to get in there.
My company got a little tired of having to jump through hoops to use the 317 grades of stainless steel...