Hello,
I am an environmental engineer(chemical eng. based)and have some structural questions:
1. Are there some rule of thumb for determining thickness of concrete wall and weight of bar in it , in a water (or waste water)storage tank?
2.What is the "break point" capacity for building wate tank in steel or concrete ?
Thanks
I am an environmental engineer(chemical eng. based)and have some structural questions:
1. Are there some rule of thumb for determining thickness of concrete wall and weight of bar in it , in a water (or waste water)storage tank?
2.What is the "break point" capacity for building wate tank in steel or concrete ?
Thanks





RE: concrete water tank
The rebar quantity will be in the region of 120 to 140kg per cubic metre of concrete cast in the walls.
Regards
Andy Machon