How to produce band saw blade from strip steel?
How to produce band saw blade from strip steel?
(OP)
Could you help me please?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
How to produce band saw blade from strip steel?
|
RE: How to produce band saw blade from strip steel?
Cut it with a laser or punch it out. Swage it. Adjust temper.
tom
RE: How to produce band saw blade from strip steel?