INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Commercial design

Commercial design

Commercial design

(OP)
Can anyone recommend some good design aides/books for commercial design engineering?

RE: Commercial design

can you define "commercial design engineering " and what field (i.e. civil, structural, mechanical or electrical)

RE: Commercial design

(OP)
I am a structural engineer.  Most of my experience is in heavy industry, such as steel mills.  I am looking for reference materials on commercial design standards for such things as retail buildings, restaurants and office buildings.

RE: Commercial design

UBC

RE: Commercial design

(OP)
I have already looked at the various building codes.  I also just bought a copy of Architectural Graphic Standards, which is very useful.  Are there any other suggestions out there?  It never hurts to have too many resources.

RE: Commercial design

You may look at "Floor vibrations due to human activity" Steel design guide series # 11 (AISC).
Commercial buildings with spans 40-50 feet will require vibration check.

RE: Commercial design

U can Consult a book"Design of Concrete Structures" by Nilson

Shahid

RE: Commercial design

You may want to check out:

Building Construction Details - Practical Drawings by Hans Banz ISBN 0-442-21330-1 or

Construction Details for Commercial Buildings - A Graphics File for Architects

RE: Commercial design

Sorry, the second text is by Glenn Wiggins and the ISBN is 0-8230-0927-0

RE: Commercial design

(OP)
Thanks for all of the great suggestions

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources