INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME SEC VIII Div 1 Appendix 31

ASME SEC VIII Div 1 Appendix 31

ASME SEC VIII Div 1 Appendix 31

(OP)
Hello

Appendix clause 31-4 of ASME SEC VIII Div 1 specifies that welding shall be limited to SAW and SMAW whereas the table 31.2 gives composition for GTAW and GMAW weld metal.

Is this an inconsistency? or is there some other meaning to this?

RE: ASME SEC VIII Div 1 Appendix 31

Re-read 31-4(a) says SAW or SMAW for 3Cr-1Mo-1/4V-Ti-b material ONLY.

RE: ASME SEC VIII Div 1 Appendix 31

(OP)
Thankyou. I realised i was refering 1998 addenda. On checking the 2001 addenda the inconsistency(it was an inconsistency after all) was found to  have been rectified.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources