Notching the Bending Zones - Sheet Metal
Notching the Bending Zones - Sheet Metal
(OP)
Just wondering if anyone has a formula or rule of thumb for notching the bending zones in sheet metal in order to create a closed corner when forming sheet metal on a press brake. How do you calculate your notch size and corner relief?
Thanks
Thanks





RE: Notching the Bending Zones - Sheet Metal
radius of relief = 5 x t.
RE: Notching the Bending Zones - Sheet Metal
Flores