INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

UK Material BS3602/35 - Smls Pipe?

UK Material BS3602/35 - Smls Pipe?

UK Material BS3602/35 - Smls Pipe?

(OP)
Does anyone know the pipe spec (Chemical and mechanical properties)?

RE: UK Material BS3602/35 - Smls Pipe?

chemical composition:
  Carbon                         0.350         0.350
  Manganese                      0.700         1.100
  Phosphorus                     0.050         0.050
  Sulfur                         0.0500        0.0500

mechanical properties:
  Tensile Strength     :    min.     480.0 MPa
  Yield Strength       :    min.       275 MPa
  Elongation           :    min.        20 %

similar materials:
1.0432     DIN      2528            Germany             
C21        DIN      2528            Germany             
35         BS       3602            Great Britain       
60         ASTM     A181            USA                 
70         ASTM     A181            USA                 
WP12 CL2   ASTM     A234            USA                 

thats abou all what the "atlas of world steels" has to say about it...
hth,
chris

RE: UK Material BS3602/35 - Smls Pipe?

(OP)
Thanks so much for your quick reply, phex! BTW, can you advise the edition and publisher for "atlas of world steels" ?

RE: UK Material BS3602/35 - Smls Pipe?

it's a piece of software running here on my company's computers...

it's made by "Eagle International Software" and is accurate as of 1997 (no comments please ;)

you should contact them directly for further info

phex

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources