INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Grinding Iconel in centerless machines

Grinding Iconel in centerless machines

Grinding Iconel in centerless machines

(OP)
Hi everyone. We are starting a develop of valves with iconel head, the problem here is get the best parameters for grinding this kind of material, Does anyone have any idea of the problem we will have doing our job??

RE: Grinding Iconel in centerless machines

Hector,
I'm working with inconel for some time. Which kind of process are you developing?

RE: Grinding Iconel in centerless machines

We have had a very good experience in using high-porous vitrified CBN wheels for grinding Inconel. These wheels do not clog and grind a way cooler. Contact me for more detailes. gurinovich@abrazive.spb.ru

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources