INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME SA-350-LF2

ASME SA-350-LF2

ASME SA-350-LF2

(OP)
Can anybody supply me with the chemical composition and mechanical properties for ASME SA- 350-LF2 or ASTM A-350.

RE: ASME SA-350-LF2

Carbon, max 0.30; Manganese 0.60¨C1.35; Phosphorus,max
0.035; Sulfur, max 0.040; Silicon 0.15¨C0.30; Nickel 0.40 max; Chromium 0.30 max; Molybdenum 0.12 max; Copper 0.40 max; Columbium 0.02 max; Vanadium 0.05 max.

Tensile strength, 70¨C95 ksi; Yield strength, min, 36 ksi.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources