INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What Spec for coupler material?

What Spec for coupler material?

What Spec for coupler material?

(OP)
Hi,

I want to couple an F1554 GR 105 (A687) anchor bolt to a swedged rod.  I need to specify material for the coupler.  I was planning on giving a length, OD and material.  I would prefer 50 ksi steel or higher.  Initially I was thinking A572 GR 50, but then realized that this probably isn't appropriate for a threaded coupler.  Can anyone point me to an ASTM spec?

Thanks,
Randy

RE: What Spec for coupler material?

Consider SAE 1008 steel, use a length twice the full engagement length and zinc plate per ASTM B 633.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources