INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Is QQZ-325-C obsolete?

Is QQZ-325-C obsolete?

Is QQZ-325-C obsolete?

(OP)
That's all- - -argument here if it is or isn't..
We should use B633...no??
thank you much..
rube

RE: Is QQZ-325-C obsolete?

QQ-Z-325C,ZINC COATING, ELECTRODEPOSITED has been cancelled.  It has been superceded by ASTM B 633.  A good website to check on the status on specifications such as this one is called ASSIST.

http://assist.daps.dla.mil/online/start/

After entering the site, click on the "Quick Search" button on the left side of the screen.  There is no need to join or to login to the site.  In the Tell us what you want screen, type in the spec you're interested in the Document ID box and the program will do the rest.

Tony D.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources