INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

young modulus vs temp

young modulus vs temp

young modulus vs temp

(OP)
Hi,
How I can use the function Young modulus vs temperature E=E(t)in the defining of the isotropic material (Nastran for Windows)?
With a lot of thanks,
Krzyszof

RE: young modulus vs temp

The modulus of elasticity of structural steel (E) is approximately 29,000 ksi at 70 deg F. It decreases linearly to about 25,000 ksi at 900 deg F and them begins to drop at an increasing rate at higher temperatures.

So it material dependent. Find numbers for material in question and make function.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources