INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AAL Overhead Conductor

AAL Overhead Conductor

AAL Overhead Conductor

(OP)
Can someone indicate the capacity of a 4/0 AWG AAL conductor, I cannot find AAL data.

Thanks

RE: AAL Overhead Conductor

Suggestion: Visit
http://www.caiso.com/docs/2000/02/08/2000020815423814921.pdf
for more info on AAL usage
and Reference:
1. Table 4-22 Aluminum Conductors on page 4-64
4/0 "Oxlip"
0.1663 in**2
365 A current carrying capacity (under certain constraints, e.g. conductor temperature rise 40°C over 40°C ambient, 2ft/sec crosswind, and emissivity factor of 0.5 without sun)
7 x 0.1739 number and diameter of wires, in
0.522 conductor diameter, in
3830 rated strength, lb
198.7 nominal weight in lb per 1000'
etc.
Also, clarify a word "capacity" in your posting.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources