INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Bolts to be used with weathering steel in Europe

Bolts to be used with weathering steel in Europe

Bolts to be used with weathering steel in Europe

(OP)
I’m trying to use atmospheric corrosion resistant steel in the design of a bridge in Spain.

I think that in USA Type 3 HS bolts are specified to be used with that kind of steel, and that Type 3 bolts are made out of weathering steel also.

But in Europe I have not found a similar specification. I have asked several steel fabricators and they said me that in Europe are used with weathering steel the same kind of bolts that are used with carbon structural steels.

Is that true? Can anybody help in telling me any reference on that topic?

Thanks.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources