INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Solubility of Ferro oxide (Fe2O3) in water Vs the pH

Solubility of Ferro oxide (Fe2O3) in water Vs the pH

Solubility of Ferro oxide (Fe2O3) in water Vs the pH

(OP)
Hi every body

It's will very appreciate if  somme one can tell me the solubility of Ferro oxide (Fe2O3) in water acid to basic (pH from 1 to 14)

Many thanks

RE: Solubility of Ferro oxide (Fe2O3) in water Vs the pH

Do you really want the solubility of Fe2O3?  This dissolves very slowly except in strong acids, and dissociates upon dissolution.

There are links for the solubility of metals (including Fe+3) as a function of pH in Thread161-50054

The solubility of Fe+3 can also be calculated as a function of pH from the solubility product, Ksp, of Fe(OH)3.

Ksp, Fe(OH)3 = [Fe+3][OH-]3 = 6 x 10-38,

so [Fe+3] = Ksp/[OH-]3, moles/Liter

and of course [OH-] = 10-[14 – pH]

RE: Solubility of Ferro oxide (Fe2O3) in water Vs the pH

(OP)
Thanks kenvlach !  Jeffrop

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources